MCQOPTIONS
Saved Bookmarks
This section includes 1232 Mcqs, each offering curated multiple-choice questions to sharpen your Electrical Engineering knowledge and support exam preparation. Choose a topic below to get started.
901. |
Surface decarburisation in steels in cold working . |
A. | does not occurs |
B. | occurs |
Answer» B. occurs | |
902. |
Stacking fault is type of defect |
A. | point |
B. | line |
C. | volume |
D. | surface |
Answer» E. | |
903. |
Stacking fault energies are in the range of |
A. | 0.01-0.1 j/m2 |
B. | 0.01-0.1 j/cm2 |
C. | 0.1-10 j/m2 |
D. | 0.1-10 j/m2 |
Answer» B. 0.01-0.1 j/cm2 | |
904. |
Square brackets are used to represent crystallographic |
A. | point location |
B. | direction |
C. | plane |
D. | none of the above |
Answer» C. plane | |
905. |
slip plane orientation after grain boundary |
A. | by pass |
B. | crosses |
C. | change |
D. | none of the above |
Answer» D. none of the above | |
906. |
Slip systems having two types one is glide & another one is |
A. | climb |
B. | slip |
C. | twinns |
D. | none of the above |
Answer» B. slip | |
907. |
Sharp break in dislocation line that is in slip plane . |
A. | jog |
B. | kink |
C. | either jog or kink |
D. | none |
Answer» C. either jog or kink | |
908. |
screw dislocations includes |
A. | tension lattice strain |
B. | compression lattice strain |
C. | shear lattice strain |
D. | all |
Answer» D. all | |
909. |
screw dislocations have burger vector for dislocation line |
A. | perpendicul ar |
B. | parallel |
C. | inclined |
D. | first perpendicul ar then parallel |
Answer» B. parallel | |
910. |
Schottky-defect in ceramic material is |
A. | interstitial impurity |
B. | vacancy- interstitial pair of cations |
C. | pair of nearby cation and anion vacancies |
D. | substitution al impurity |
Answer» D. substitution al impurity | |
911. |
Schottky-defect is of this type. |
A. | point |
B. | line |
C. | volume |
D. | surface |
Answer» B. line | |
912. |
Schottky defect found in |
A. | metal |
B. | non-metal |
C. | ionic |
D. | plastics |
Answer» D. plastics | |
913. |
Schottky defect have missing of |
A. | cation |
B. | anion |
C. | electron |
D. | both a&b |
Answer» E. | |
914. |
Recrystallization rate varies in the following manner with temperature |
A. | linearly increasing |
B. | linearly decreasing |
C. | exponential |
D. | logarithmic |
Answer» D. logarithmic | |
915. |
Repeatable entity of a crystal structure is known as |
A. | crystal |
B. | lattice |
C. | unit cell |
D. | miller indices |
Answer» D. miller indices | |
916. |
Requirement for cross-slip movement of dislocation |
A. | preferred slip plane |
B. | preferred slip direction |
C. | no preferred slip plane |
D. | no preferred slip direction |
Answer» D. no preferred slip direction | |
917. |
Round brackets are used to represent crystallographic |
A. | point location |
B. | direction |
C. | plane |
D. | none of the above |
Answer» D. none of the above | |
918. |
Recrystallisation temperature of Iron is ……….. |
A. | 727 °c |
B. | 775 °c |
C. | 800 °c |
D. | 700 °c |
Answer» B. 775 °c | |
919. |
Positive screw dislocation is represented by |
A. | â”´ |
B. | 0 |
C. | ┬ |
Answer» B. 0 | |
920. |
Oxidation of metals occurs during cold working. |
A. | true |
B. | false |
Answer» C. | |
921. |
Poor surface finish in………process |
A. | cold working |
B. | hot working |
C. | casting |
D. | welding |
Answer» C. casting | |
922. |
Plastic deformation results from the following. |
A. | edge dislocation |
B. | screw dislocations |
C. | mixed dislocations |
D. | all of the above |
Answer» E. | |
923. |
No.of atoms in FCCstructure are ….. |
A. | 2 |
B. | 1 |
C. | 4 |
D. | 5 |
Answer» D. 5 | |
924. |
No. of atoms in Body-Centered Cubic structure are ….. |
A. | 1 |
B. | 2 |
C. | 4 |
D. | 6 |
Answer» C. 4 | |
925. |
No. of atoms in hexagon close packed structure are ….. |
A. | 1 |
B. | 2 |
C. | 4 |
D. | 6 |
Answer» E. | |
926. |
Minimum number of slip systems that must be operative during plastic deformation |
A. | 3 |
B. | 4 |
C. | 5 |
D. | 6 |
Answer» D. 6 | |
927. |
Miller indices of the line of intersection of (⎯ 1⎯ 11) and (110) are |
A. | [110] |
B. | [101] |
C. | [10-1] |
D. | [-110] |
Answer» E. | |
928. |
Material having CRSS shows large plastic deformation |
A. | high |
B. | low |
C. | constant |
D. | none of the above |
Answer» C. constant | |
929. |
Material having cohesive strength shows large plastic deformation |
A. | high |
B. | low |
C. | constant |
D. | none of the above |
Answer» B. low | |
930. |
Ligancy number for HCP is |
A. | 6 |
B. | 12 |
C. | 4 |
D. | 8 |
Answer» C. 4 | |
931. |
Lattice structure represents arrangement of unit cells in |
A. | 2- dimensional axes system |
B. | 3- dimensional axes system |
C. | orthographi c system |
D. | none of the above |
Answer» C. orthographi c system | |
932. |
It is a type of Twin |
A. | annealing |
B. | tempering |
C. | normalising |
D. | hardening |
Answer» B. tempering | |
933. |
Inter atomic distance is more                   the dislocation line in negative edge dislocation |
A. | above |
B. | below |
C. | right side of |
D. | left side of |
Answer» B. below | |
934. |
In vacancy point defects, stress field produced in the vicinity. |
A. | tension |
B. | shear |
C. | compression |
D. | all |
Answer» B. shear | |
935. |
In hot working microstructure is |
A. | distorted |
B. | equiaxed |
C. | refined |
D. | both b & c |
Answer» E. | |
936. |
Inter atomic distance is more                   the dislocation line in positive edge dislocation |
A. | above |
B. | below |
C. | right side of |
D. | left side of |
Answer» C. right side of | |
937. |
Indexing or designation in a unit cell can be done for a particular |
A. | point location |
B. | direction |
C. | plane |
D. | all of the above |
Answer» E. | |
938. |
In hot working force required is than cold working |
A. | greater |
B. | less |
C. | equal |
D. | can’t say |
Answer» C. equal | |
939. |
In geometrical softening, at the beginning λ is |
A. | less than 45° |
B. | more than 35° |
C. | more than 45° |
D. | less than 35° |
Answer» C. more than 45° | |
940. |
In geometrical hardening, at the beginning λ is |
A. | less than 45° |
B. | more than 35° |
C. | more than 45° |
D. | less than 35° |
Answer» B. more than 35° | |
941. |
In FCC, the lattice parameter (a) is |
A. | (4/√3) r |
B. | 4/√3 r |
C. | (4/√2) r |
D. | 4/√2 r |
Answer» D. 4/√2 r | |
942. |
In Cold work,strength |
A. | increases |
B. | decreases |
C. | remains same |
D. | none |
Answer» B. decreases | |
943. |
In cold working, due to strain hardening ductility of metal |
A. | increases |
B. | decreases |
C. | remains same |
D. | can’t say |
Answer» C. remains same | |
944. |
In cold working, electrical resistance |
A. | increases |
B. | decreases |
C. | remains same |
D. | can’t say |
Answer» B. decreases | |
945. |
In cold working, corrosion resistance |
A. | increases |
B. | decreases |
C. | remains same |
D. | can’t say |
Answer» C. remains same | |
946. |
In climb, the dislocation moves of the surface |
A. | in , glide |
B. | out, glide |
C. | in, twinns |
D. | out, twinns |
Answer» C. in, twinns | |
947. |
In case of polycrystalline materials regeneration rate of dislocations |
A. | increases |
B. | decreases |
C. | remains same |
D. | can’t say |
Answer» B. decreases | |
948. |
In BCC, the lattice parameter (a) is |
A. | (4/√3) r |
B. | 4/√3 r |
C. | (4/√2) r |
D. | 4/√2 r |
Answer» B. 4/√3 r | |
949. |
If the deformation is carried out below RCT, it is |
A. | cold working |
B. | hot working |
C. | both a and b |
D. | none |
Answer» B. hot working | |
950. |
If the deformation is carried out above RCT, it is |
A. | cold working |
B. | hot working |
C. | both a and b |
D. | none |
Answer» C. both a and b | |