				This section includes 20 Mcqs, each offering curated multiple-choice questions to sharpen your Prestressed Concrete Structures knowledge and support exam preparation. Choose a topic below to get started.
| 1. | How many wedges are considered in the case of torpedo splices? | 
| A. | 3 | 
| B. | 4 | 
| C. | 5 | 
| D. | 2 | 
| Answer» B. 4 | |
| 2. | In thermo electric pre stressing, the elongation is observed in case of ___________ | 
| A. | Bar after cooling | 
| B. | Bar after heating | 
| C. | Bar after anchoring | 
| D. | Simple bar | 
| Answer» C. Bar after anchoring | |
| 3. | The estimation of the current, voltage and power requirements of the transformer are for ___________ | 
| A. | Theoretical equations | 
| B. | Empirical relations | 
| C. | Global relations | 
| D. | Quadratic equations | 
| Answer» C. Global relations | |
| 4. | The tensioning of oval section ribbed wires with an ultimate tensile strength was adopted in ___________ | 
| A. | Germany | 
| B. | France | 
| C. | Switzerland | 
| D. | Britain | 
| Answer» B. France | |
| 5. | The thermo electric pre stressing is also used in ___________ | 
| A. | Pre-block units | 
| B. | Pre-cast units | 
| C. | Pre-beam units | 
| D. | Pre-anchorage units | 
| Answer» C. Pre-beam units | |
| 6. | In which place thermo electric pre stressing found to be more economical? | 
| A. | Canada | 
| B. | USSR | 
| C. | France | 
| D. | Switzerland | 
| Answer» C. France | |
| 7. | The thermo electric pre stressing, initial stress in tendons ranges between ___________ | 
| A. | 500-600n/mm2 | 
| B. | 200-300n/mm2 | 
| C. | 100-150n/mm2 | 
| D. | 600-800n/mm2 | 
| Answer» B. 200-300n/mm2 | |
| 8. | The period of cooling in thermo electric pre stressing is observed as ___________ | 
| A. | 20-30 minutes | 
| B. | 12-15 minutes | 
| C. | 5-10 minutes | 
| D. | 15-20 minutes | 
| Answer» C. 5-10 minutes | |
| 9. | In thermo electric pre stressing, heating the bars is done to a temperature of ___________ | 
| A. | 300-400degrees | 
| B. | 500-600degrees | 
| C. | 200-300degrees | 
| D. | 150-450degrees | 
| Answer» B. 500-600degrees | |
| 10. | The method of pre stressing by heated tendons, achieved by passing an electric current is known as ___________ | 
| A. | Chemical pre stressing | 
| B. | Thermo electric pre stressing | 
| C. | Dynamic pre stressing | 
| D. | Thermo blasting pre stressing | 
| Answer» C. Dynamic pre stressing | |
| 11. | HOW_MANY_WEDGES_ARE_CONSIDERED_IN_CASE_OF_TORPEDO_SPLICES??$ | 
| A. | 3 | 
| B. | 4 | 
| C. | 5 | 
| D. | 2 | 
| Answer» B. 4 | |
| 12. | In thermo electric pre stressing, the elongation is observed in case of? | 
| A. | Bar after cooling | 
| B. | Bar after heating | 
| C. | Bar after anchoring | 
| D. | Simple bar | 
| Answer» C. Bar after anchoring | |
| 13. | The estimation of the current, voltage and power requirements of the transformer are for? | 
| A. | Theoretical equations | 
| B. | Empirical relations | 
| C. | Global relations | 
| D. | Quadratic equations | 
| Answer» C. Global relations | |
| 14. | The tensioning of oval section ribbed wires with an ultimate tensile strength was adopted in: | 
| A. | Germany | 
| B. | France | 
| C. | Switzerland | 
| D. | Britain | 
| Answer» B. France | |
| 15. | The thermo electric pre stressing is also used in: | 
| A. | Pre-block units | 
| B. | Pre-cast units | 
| C. | Pre-beam units | 
| D. | Pre-anchorage units | 
| Answer» C. Pre-beam units | |
| 16. | In which place thermo electric pre stressing found to be more economical: | 
| A. | Canada | 
| B. | USSR | 
| C. | France | 
| D. | Switzerland | 
| Answer» C. France | |
| 17. | The thermo electric pre stressing, initial stress in tendons ranges between: | 
| A. | 500-600n/mm<sup>2</sup> | 
| B. | 200-300n/mm<sup>2</sup> | 
| C. | 100-150n/mm<sup>2</sup> | 
| D. | 600-800n/mm<sup>2</sup> | 
| Answer» B. 200-300n/mm<sup>2</sup> | |
| 18. | The period of cooling in thermo electric pre stressing is observed as: | 
| A. | 20-30 minutes | 
| B. | 12-15 minutes | 
| C. | 5-10 minutes | 
| D. | 15-20 minutes | 
| Answer» C. 5-10 minutes | |
| 19. | In thermo electric pre stressing, heating the bars is done to a temperature of: | 
| A. | 300-400degrees | 
| B. | 500-600degrees | 
| C. | 200-300degrees | 
| D. | 150-450degrees | 
| Answer» B. 500-600degrees | |
| 20. | The method of pre stressing by heated tendons, achieved by passing an electric current is known as: | 
| A. | Chemical pre stressing | 
| B. | Thermo electric pre stressing | 
| C. | Dynamic pre stressing | 
| D. | Thermo blasting pre stressing | 
| Answer» C. Dynamic pre stressing | |