1. |
What percentage of powered ferrosilicon is mixed with sodium silicate bonded sand in Nishiyama process? |
A. | 1% |
B. | 2% |
C. | 3% |
D. | 4% |
Answer» C. 3% | |
2. |
Silica gel is formed when sodium bicarbonate reacts with carbon monoxide. |
A. | True |
B. | False |
Answer» C. | |
3. |
Which of the following core cannot be classified under the shape and position of the core? |
A. | Balanced core |
B. | Ram up core |
C. | Shell core |
D. | Horizontal core |
Answer» D. Horizontal core | |
4. |
Which of the following will not be classified under the type of core hardening process employed? |
A. | Nishiyama process |
B. | Ram up core |
C. | Furan no-bake system |
D. | Cold set process |
Answer» C. Furan no-bake system | |
5. |
Which of the following core cannot be classified by the nature of core material employed? |
A. | Dry sand core |
B. | Shell core |
C. | Sodium silicate core |
D. | Oil bonded core |
Answer» B. Shell core | |
6. |
WHAT_PERCENTAGE_OF_POWERED_FERROSILICON_IS_MIXED_WITH_SODIUM_SILICATE_BONDED_SAND_IN_NISHIYAMA_PROCESS??$ |
A. | 1% |
B. | 2% |
C. | 3% |
D. | 4% |
Answer» C. 3% | |
7. |
What percentage of clay content is required in furan-no-bake system? |
A. | Less than 0.3% |
B. | Less than 0.4% |
C. | Less than 0.5% |
D. | Less than 0.6% |
Answer» D. Less than 0.6% | |
8. |
Silica gel is formed when sodium bicarbonate reacts with carbon monoxide? |
A. | True |
B. | False |
Answer» C. | |
9. |
Sodium silicate reacts with carbon dioxide to give what? |
A. | Sodium dichromate |
B. | Sodium sulphide |
C. | Sodium bicarbonate |
D. | Sodium carbonate |
Answer» E. | |
10. |
In hot box process, core box is heated up to what temperature? |
A. | 220°F – 300°F |
B. | 250°F – 320°F |
C. | 350°F – 500°F |
D. | 420°F – 550°F |
Answer» D. 420¬¨¬®‚Äö√†√ªF ‚Äö√Ñ√∂‚àö√ë‚àö¬® 550¬¨¬®‚Äö√†√ªF | |
11. |
In resin bond cores, the core is baked at what temperature? |
A. | 275°F – 390°F |
B. | 375°F – 450°F |
C. | 485°F – 645°F |
D. | 775°F – 880°F |
Answer» C. 485¬¨¬®‚Äö√†√ªF ‚Äö√Ñ√∂‚àö√ë‚àö¬® 645¬¨¬®‚Äö√†√ªF | |
12. |
Which of the following cores are produced by mixing silica? |
A. | Green sand cores |
B. | Dry sand cores |
C. | Oil bonded cores |
D. | Resin bonded cores |
Answer» D. Resin bonded cores | |
13. |
Which of the following core cannot be classified under shape and position of the core? |
A. | Balanced core |
B. | Ram up core |
C. | Shell core |
D. | Horizontal core |
Answer» D. Horizontal core | |
14. |
Which of the following will not be classified under type of core hardening process employed? |
A. | Nishiyama process |
B. | Ram up core |
C. | Furan no-bake system |
D. | Cold set process |
Answer» C. Furan no-bake system | |
15. |
Which of the following core cannot be classified by nature of core material employed? |
A. | Dry sand core |
B. | Shell core |
C. | Sodium silicate core |
D. | Oil bonded core |
Answer» B. Shell core | |