MCQOPTIONS
Saved Bookmarks
This section includes 14 Mcqs, each offering curated multiple-choice questions to sharpen your Engineering Materials Metallurgy knowledge and support exam preparation. Choose a topic below to get started.
1. |
__________ solders are used for glass-to-glass and glass-to-metal soldering. |
A. | Lead-silver |
B. | Tin-zinc |
C. | Cadmium-zinc |
D. | Indium-tin |
Answer» E. | |
2. |
Aluminum can be joined to another aluminum with the use of ________ solder. |
A. | Lead-silver |
B. | Indium-tin |
C. | Cadmium-silver |
D. | Fusible alloy |
Answer» D. Fusible alloy | |
3. |
Addition of ___________ increases the mechanical properties of a tin-lead solder. |
A. | Bismuth |
B. | Tellurium |
C. | Antimony |
D. | Molybdenum |
Answer» D. Molybdenum | |
4. |
Which of the following filler metals is used in the electrical industry? |
A. | BAG-1 |
B. | BAG-3 |
C. | BAG-5 |
D. | BAG-6 |
Answer» D. BAG-6 | |
5. |
___________SOLDERS_ARE_USED_FOR_GLASS-TO-GLASS_AND_GLASS-TO-METAL_SOLDERING.?$ |
A. | Lead-silver |
B. | Tin-zinc |
C. | Cadmium-zinc |
D. | Indium-tin |
Answer» E. | |
6. |
Aluminum can be joined to another aluminum with the use of ________ solder? |
A. | Lead-silver |
B. | Indium-tin |
C. | Cadmium-silver |
D. | Fusible alloy |
Answer» D. Fusible alloy | |
7. |
Addition of ___________ increases the mechanical properties of a tin-lead solder? |
A. | Bismuth |
B. | Tellurium |
C. | Antimony |
D. | Molybdenum |
Answer» D. Molybdenum | |
8. |
What is the solidus temperature of tin-lead solders? |
A. | 183 |
B. | 297 |
C. | 444 |
D. | 604 |
Answer» B. 297 | |
9. |
Tin-zinc solders are used for joining __________ |
A. | Aluminum |
B. | Zinc |
C. | Copper |
D. | Glass |
Answer» B. Zinc | |
10. |
Which of the following filler metals is used for carbide tip brazing? |
A. | BAG-1 |
B. | BAG-4 |
C. | BAG-8 |
D. | BAG-18 |
Answer» C. BAG-8 | |
11. |
Nickel filler metals are heat resistant up to ________ in short time service. |
A. | 610<sup>o</sup>C |
B. | 982<sup>o</sup>C |
C. | 1204<sup>o</sup>C |
D. | 1666<sup>o</sup>C |
Answer» D. 1666<sup>o</sup>C | |
12. |
Which of the following filler metals is used in electrical industry? |
A. | BAG-1 |
B. | BAG-3 |
C. | BAG-5 |
D. | BAG-6 |
Answer» D. BAG-6 | |
13. |
Copper and aluminum can be joined by brazing when _________ alloy is used. |
A. | Copper-zinc |
B. | Aluminum-silicon |
C. | Copper-tellurium |
D. | Aluminum-zinc |
Answer» C. Copper-tellurium | |
14. |
The liquid temperature of the filler metal used in brazing is _________ |
A. | 150<sup>o</sup>C |
B. | 427<sup>o</sup>C |
C. | 723<sup>o</sup>C |
D. | 1000<sup>o</sup>C |
Answer» C. 723<sup>o</sup>C | |