Explore topic-wise MCQs in Chemical Engineering.

This section includes 568 Mcqs, each offering curated multiple-choice questions to sharpen your Chemical Engineering knowledge and support exam preparation. Choose a topic below to get started.

301.

Skull is not formed on the carbon blocks in the hearth of a blast furnace, when it becomes cold, because of its

A. non-wetting characteristic.
B. high thermal conductivity.
C. high crushing strength.
D. none of these.
Answer» B. high thermal conductivity.
302.

Epoxy resin is a polymer containing two or more following groups called epoxide group or ethoxyline group. It is a

A. polyamide & an elastomer.
B. good adhesive.
C. surface coating agent.
D. both (b) and (c).
Answer» E.
303.

Epoxy resins (i.e., epoxide polymers)

A. A
B. B
C. C
D. D
Answer» C. C
304.

PCE value (Segar cone) of superduty refractories is more than 33, which is equivalent to a temperature of __________ °C.

A. 1520
B. 1630
C. 1670
D. 1730
Answer» E.
305.

Spalling of silica bricks occurs due to abrupt volume changes, when it is cooled below a temperature of __________ °C.

A. 770
B. 570
C. 270
D. 70
Answer» D. 70
306.

Pyrometric cone equivalent (PCE) value (Segar cone) of 'superduty refractories' is more than 33 which corresponds to a temperature of __________ °C.

A. 1520
B. 1630
C. 1670
D. 1730
Answer» E.
307.

Refractoriness of a typical silica brick corresponds to Segar cone number, '32', which is equivalent to a temperature of __________ °C.

A. 1380
B. 1520
C. 1710
D. 1915
Answer» D. 1915
308.

Which of the following is not an acidic refractory?

A. Silica bricks
B. Fireclay bricks
C. Bauxite bricks
D. Magnesia bricks
Answer» E.
309.

Which brick undergoes maximum shrinkage on drying?

A. Tar bonded dolomite bricks
B. Fireclay bricks
C. Magnesite bricks
D. Chromite bricks
Answer» C. Magnesite bricks
310.

Which one contains maximum percentage of Al2O₃ ?

A. Firebrick
B. Sillimanite
C. Magnesite
D. Aluminous firebrick
Answer» C. Magnesite
311.

Hot blast main (carrying air at 1000°C) in blast furnace are lined with __________ bricks.

A. Silica
B. Fireclay
C. Magnesite
D. Zirconia
Answer» C. Magnesite
312.

Which one expands on heating?

A. Silica bricks
B. Fireclay bricks
C. Both A & B
D. Neither A nor B
Answer» B. Fireclay bricks
313.

Which is a basic refractory?

A. Fireclay
B. Silica
C. Chrome magnesite
D. None of these
Answer» D. None of these
314.

Which of the following impurities reduces the refractoriness of magnesite bricks?

A. Al2O₃
B. CaO
C. SiO₂
D. All of the above
Answer» E.
315.

What is Thoria?

A. Thoria Has high fusion temperature (> 3000°C) but poor resistance to thermal shock
B. Thoria Has high resistance to basic slags
C. Which is expensive & radioactive, is used in crucibles for melting high purity metals
D. All of the above
Answer» E.
316.

Which form of silica has the highest specific gravity?

A. Quartz
B. Cristobalite
C. Tridymite
D. All of the above
Answer» B. Cristobalite
317.

Silica bricks have low spalling resistance below 600°C, due to its

A. Very high thermal conductivity
B. High co-efficient of expansion upto this temperature
C. High thermal diffusivity
D. Low refractoriness
Answer» C. High thermal diffusivity
318.

Which of the following bricks should not be used, if the furnace is to be used intermit-tantly?

A. Firebricks
B. Silica bricks
C. Silicon carbide bricks
D. Sillimanite
Answer» C. Silicon carbide bricks
319.

Which is not an acidic refractory?

A. Silica
B. Fireclay
C. High alumina refractory
D. Carbon black
Answer» E.
320.

Which of the following is not a neutral refractory?

A. Silicon carbide
B. Magnesite
C. Chromite
D. Graphite
Answer» C. Chromite
321.

Cold crushing strength of fireclay bricks is about __________ kgf/cm².

A. 50-100
B. 100-150
C. 200-400
D. 500-1000
Answer» D. 500-1000
322.

Which of the following does not occur during firing/burning of refractories?

A. Removal of water of hydration
B. Vitrification
C. Decrease in crushing strength
D. Development of stable mineral form
Answer» D. Development of stable mineral form
323.

Refractoriness/fusion points of 'superduty' refractories is __________ °C.

A. 1520-1630
B. 1630-1670
C. > 1730
D. > 2000
Answer» D. > 2000
324.

SiO₂ percentage in firebrick is about

A. 35-40
B. 55-60
C. 80-85
D. >94
Answer» C. 80-85
325.

Beryllia (which is used in making crucibles for melting uranium & thorium) is superior to alumina in all respects for high temperature (> 1900°C ) use, except

A. Cost
B. Electrical conductivity
C. Thermal conductivity
D. Fusion point
Answer» B. Electrical conductivity
326.

Silliminite (Al2O₃.SiO₂) refractory, which is a neutral refractory, is not used in

A. Pottery furnace
B. Glass melting furnace
C. Crucibles
D. Gas retorts
Answer» E.
327.

Which of the following has the lowest electrical resistivity?

A. Graphite
B. Fireclay
C. Alumina
D. Zircon
Answer» B. Fireclay
328.

Which is not a high alumina refractory?

A. Mullite
B. Corrundum
C. Bauxite
D. Dolomite
Answer» E.
329.

The linear thermal expansion of __________ bricks upto 1000 °C is very low of the order of ≤ 0.5 percent.

A. Fireclay
B. Silica
C. Magnesite
D. Corundum
Answer» B. Silica
330.

Which one contains minimum percentage of SiO₂?

A. Firebrick
B. Sillimanite
C. Semi-silica
D. Aluminous firebrick
Answer» C. Semi-silica
331.

__________ nozzles are used in continuous casting of steel,

A. Zircon
B. Thoria
C. Carborundum
D. Beryllia
Answer» B. Thoria
332.

Which refractory must have controlled atmosphere (temperature and humidity) for its safe storage?

A. Tar bonded dolomite bricks
B. Fireclay bricks
C. Mullite bricks
D. Magnesite bricks
Answer» B. Fireclay bricks
333.

Which is required in an insulating refractory?

A. High thermal conductivity
B. Low porosity
C. Both A & B
D. Neither A nor B
Answer» E.
334.

Because of its very high refractoriness of the order of __________ °C, silicon carbide refractories are used in zinc smelting furnace, muffle furnace and for supporting the wares in tunnel kilns.

A. 1800
B. 2200
C. 2400
D. 2700
Answer» E.
335.

Which furnace consumes maximum refractory annually in an integrated steel plant?

A. Soaking pit
B. Blastfurnace
C. L.D. converter
D. Coke ovens
Answer» D. Coke ovens
336.

Fusion temperature of pure silica (SiO₂) is __________ °C.

A. 1350
B. 1715
C. 2570
D. 2800
Answer» C. 2570
337.

Which is the most stable crystalline form of silica at room temperature?

A. Quartz
B. Cristobalite
C. Tridymite
D. None of these
Answer» B. Cristobalite
338.

Refractoriness under load (RUL) of fireclay bricks (under a load of 2 kg/cm² ) is __________ °C.

A. 500
B. 1000
C. >1350
D. >2000
Answer» D. >2000
339.

Which is an acidic refractory?

A. Magnesite
B. Dolomite
C. Fireclay
D. Chrome magnesite
Answer» D. Chrome magnesite
340.

Which is a neutral refractory?

A. Graphite
B. Magnesite chrome
C. Silica
D. Magnesia
Answer» B. Magnesite chrome
341.

Machine moulding of dry mixture of refractories requires a pressure of the order of __________ kg/cm².

A. 10
B. 100
C. 500
D. 1000
Answer» E.
342.

The highest melting pure oxide (m.p. > 3000°C) is

A. Thoria
B. Alumina
C. Beryllia
D. Zirconia
Answer» B. Alumina
343.

Which is the stable form of silica upto 1470°C ?

A. Quartz
B. Cristobalite
C. Tridymite
D. None of these
Answer» D. None of these
344.

Which is the stable form of silica below 870°C ?

A. Tridymite
B. Cristobalite
C. Quartz
D. None of these
Answer» D. None of these
345.

Which of the following bricks has the most close values of RUL and PCE?

A. Silica bricks
B. Fireclay bricks
C. High alumina bricks
D. Tar dolomite bricks
Answer» B. Fireclay bricks
346.

Cold crushing strength of ordinary fireclay brick is about 950 kg/cm² . On exposure to a temperature of about 1500°C, its crushing strength may come down to as low as __________ kg/cm² .

A. 450
B. 250
C. 150
D. 65
Answer» E.
347.

Maximum safe working temperature for fireclay bricks is about __________ °C.

A. 1150
B. 1300
C. 1450
D. 1550
Answer» E.
348.

Firing temperature of magnesite bricks is about __________ °C.

A. 800-1000
B. 1000-1200
C. 1600-1800
D. 2400-2600
Answer» D. 2400-2600
349.

Which is not a basic refractory?

A. Chrome magnesite
B. Magnesite
C. Dolomite
D. Silicon carbide
Answer» E.
350.

In panel test for spalling resistance, the average face temperature of panel assembly is maintained at __________ °C for 24 hours.

A. 700
B. 1000
C. 1600
D. 2000
Answer» D. 2000