MCQOPTIONS
Saved Bookmarks
This section includes 10 Mcqs, each offering curated multiple-choice questions to sharpen your Powder Metallurgy knowledge and support exam preparation. Choose a topic below to get started.
1. |
______ is carried out after sintering of self-lubricating bearings. |
A. | Sizing |
B. | Impregnation |
C. | Plating |
D. | Joining |
Answer» B. Impregnation | |
2. |
Iron base bearings are sintered at _______ |
A. | 1500-1800°C |
B. | 900-1000°C |
C. | 800-850°C |
D. | 1100-1125°C |
Answer» E. | |
3. |
Which of the following atmosphere is used for the sintering of bronze bearings? |
A. | Reducing |
B. | Oxidizing |
C. | Protective |
D. | Vacuum |
Answer» B. Oxidizing | |
4. |
The microstructure of sintered copper base self-lubricating bearing consists of ________ |
A. | pores |
B. | graphite particles |
C. | alpha phase, graphite particles |
D. | alpha phase, graphite particles, and pores |
Answer» E. | |
5. |
What is the compaction pressure range used for bronze bearings? |
A. | 775-1000 MPa |
B. | 500-800 MPa |
C. | 275-480 MPa |
D. | 200-300 MPa |
Answer» D. 200-300 MPa | |
6. |
Green density distribution is an important factor for production of porous bearings. |
A. | True |
B. | False |
Answer» B. False | |
7. |
Mixing of elemental powder is essential prior to compaction. |
A. | True |
B. | False |
Answer» B. False | |
8. |
_______ base bearings, atomized or reduced powders are employed. |
A. | Bismuth |
B. | Bronze |
C. | Iron |
D. | Tin |
Answer» D. Tin | |
9. |
Tin powder is made by _________ |
A. | Atomization |
B. | Electrolysis |
C. | Reduction |
D. | Cold stream process |
Answer» B. Electrolysis | |
10. |
_______ are bearings containing bronze or iron powder mixed with graphite. |
A. | Hydrocarbon impregnated |
B. | Oil impregnated |
C. | Plastic impregnated |
D. | Metal impregnated |
Answer» C. Plastic impregnated | |