Iron base bearings are sintered at _______..
1.
Iron base bearings are sintered at _______
A.
1500-1800°C
B.
900-1000°C
C.
800-850°C
D.
1100-1125°C
Answer» E.
Show Answer
Discussion
No Comment Found
Post Comment
Related MCQs
______ is carried out after sintering of self-lubricating bearings.
Iron base bearings are sintered at _______
Which of the following atmosphere is used for the sintering of bronze bearings?
The microstructure of sintered copper base self-lubricating bearing consists of ________
What is the compaction pressure range used for bronze bearings?
Green density distribution is an important factor for production of porous bearings.
Mixing of elemental powder is essential prior to compaction.
_______ base bearings, atomized or reduced powders are employed.
Tin powder is made by _________
_______ are bearings containing bronze or iron powder mixed with graphite.
Reply to Comment
×
Name
*
Email
*
Comment
*
Submit Reply