1.

γ form of iron is?

A. Magnetic
B. Non magnetic
C. Occurs below 768oC
D. Occurs above 1410oC
Answer» B. Non magnetic
2.

Which of the following reaction does not exhibit mushy zone in Fe-C phase diagram?

A. Eutectic reaction
B. Peritectic reaction
C. Eutectoid reaction
D. Peritectoid reaction
Answer» B. Peritectic reaction
3.

The percentage of carbon at peritectic point in Fe-C phase diagram is?

A. 2.1
B. 4.3
C. 0.83
D. 0.18
Answer» E.
4.

The percentage of carbon at eutectoid point in Fe-C phase diagram is?

A. 2.1
B. 4.3
C. 0.83
D. 0.02
Answer» D. 0.02
5.

The percentage of carbon at eutectic point in Fe-C phase diagram is?

A. 2.1
B. 4.3
C. 0.83
D. 0.02
Answer» C. 0.83
6.

The temperature (in oC) of eutectoid reaction in iron-carbon phase diagram is?

A. 1120
B. 725
C. 910
D. 820
Answer» C. 910
7.

The temperature (in oC) of eutectic reaction in iron-carbon phase diagram is?

A. 1539
B. 1493
C. 910
D. 1150
Answer» E.
8.

The temperature (in oC) of peritectic reaction in iron-carbon phase diagram is?

A. 1539
B. 1493
C. 910
D. 1175
Answer» C. 910
9.

Iron-Carbon phase diagram is a ___________

A. Unary phase diagram
B. Binary phase diagram
C. Tertiary phase diagram
D. Ternary phase diagram
Answer» C. Tertiary phase diagram
10.

The melting point of iron (in oC) is?

A. 768
B. 1535
C. 1410
D. 910
Answer» C. 1410