Which of the following impurity that causes rapid intergranular stress corrosion cracking of sensitized austenitic stainless steels in refinery operations? |
| A. | Sodium chloride |
| B. | Naphthenic acid |
| C. | Hydrogen sulfide |
| D. | Carbon dioxide |
| Answer» C. Hydrogen sulfide | |