1. |
Which of the following impurity that causes rapid intergranular stress corrosion cracking of sensitized austenitic stainless steels in refinery operations? |
A. | Sodium chloride |
B. | Naphthenic acid |
C. | Hydrogen sulfide |
D. | Carbon dioxide |
Answer» C. Hydrogen sulfide | |