In full annealing, the hypo-eutectoid steel is heated from 30 C to 50 C above the upper critical temperature and then cooled |
| A. | in still air |
| B. | slowly in the furnace |
| C. | suddenly in a suitable cooling medium |
| D. | any one of these |
| Answer» C. suddenly in a suitable cooling medium | |