1.

Differential scanning calorimetry is useful for determining the ____________

A. Melting temperature, glass transition temperature, heat of fusion etc
B. Volatilities of plasticizers and other additives
C. Quantitative determination of additives in polymers
D. Structural imperfections
Answer» B. Volatilities of plasticizers and other additives