1. |
When plates of two different thicknesses and/or widths are joined, the wider or thicker part should be reduced at the butt joint to make __________ |
A. | thickness less than smaller part, the slope being steeper than one in five |
B. | thickness greater than smaller part, the slope being steeper than one in five |
C. | thickness equal to smaller part, the slope not being steeper than one in five |
D. | thickness equal to smaller part, the slope being steeper than one in five |
Answer» D. thickness equal to smaller part, the slope being steeper than one in five | |
2. |
What is face reinforcement used in butt joint? |
A. | It is extra weld metal that makes throat dimensions greater than the thickness of the welded material |
B. | It is extra weld metal that makes the throat dimensions smaller than the thickness of the welded material |
C. | It is extra weld metal that makes the throat dimensions equal to the thickness of the welded material |
D. | It is parent metal makes that the throat dimensions smaller than the thickness of the welded material |
Answer» B. It is extra weld metal that makes the throat dimensions smaller than the thickness of the welded material | |
3. |
Which of the following are correct regarding butt joints over lap joints? |
A. | Lap joints eliminates eccentricity whereas butt joints develops eccentricity |
B. | Butt joints minimizes the size of connection |
C. | Lap joints are aesthetically pleasing over butt joints |
D. | Butt joint obtained from full penetration groove weld has 50% efficiency |
Answer» C. Lap joints are aesthetically pleasing over butt joints | |
4. |
The types of welded joints does not depend on _________ |
A. | size of members connected at joint |
B. | type of loading |
C. | area available for welding |
D. | size of weld |
Answer» E. | |
5. |
Cold cracks can be prevented by __________ |
A. | uniform heating |
B. | by use of low hydrogen electrode |
C. | faster cooling |
D. | slower cooling |
Answer» C. faster cooling | |