Explore topic-wise MCQs in Mechanical Behaviour.

This section includes 18 Mcqs, each offering curated multiple-choice questions to sharpen your Mechanical Behaviour knowledge and support exam preparation. Choose a topic below to get started.

1.

Stacking fault energy of silver is _____

A. 40 – 50 mJm-2
B. 70 – 80 mJm-2
C. 10 – 20 mJm-2
D. 20 – 30 mJm-2
Answer» E.
2.

What is the stacking sequence for FCC structure?

A. ABABAB
B. ABCABC
C. AAA
D. ABCDABCD
Answer» C. AAA
3.

High angle grain boundaries provide easy atom diffusion in a solid state.

A. True
B. False
Answer» B. False
4.

A low angle grain boundary, formed by set of _______ dislocations, is defined as twist boundary.

A. Edge
B. Mixed
C. Screw
D. Taylor
Answer» D. Taylor
5.

A low angle grain boundary formed by an array of edge dislocations is referred to as ______ boundary.

A. Tilt
B. Twin
C. Twist
D. Sub
Answer» B. Twin
6.

A_LOW_ANGLE_GRAIN_BOUNDARY,_FORMED_BY_SET_OF_________DISLOCATIONS,_IS_DEFINED_AS_TWIST_BOUNDARY.?$

A. Edge
B. Mixed
C. Screw
D. Taylor
Answer» D. Taylor
7.

What is the stacking sequence for FCC structure?$

A. ABABAB
B. ABCABC
C. AAA
D. ABCDABCD
Answer» C. AAA
8.

High_angle_grain_boundaries_provide_easy_atom_diffusion_in_a_solid_state.$

A. True
B. False
Answer» B. False
9.

Higher Stacking fault energy materials face more difficulty in cross slip and climb.

A. True
B. False
Answer» C.
10.

Stacking_fault_energy_of_silver_is______

A. 40 – 50 mJm<sup>-2</sup>
B. 70 – 80 mJm<sup>-2</sup>
C. 10 – 20 mJm<sup>-2</sup>
D. 20 – 30 mJm<sup>-2</sup>
Answer» E.
11.

A low angle grain boundary formed by an array of edge dislocations is referred to as ______ boundary?

A. Tilt
B. Twin
C. Twist
D. Sub
Answer» B. Twin
12.

Mechanical twins are commonly observed in _____ while annealing twins are observed in ______

A. FCC, BCC
B. BCC, HCP
C. FCC, HCP
D. HCP, FCC
Answer» E.
13.

Nital etchant is used for revealing microstructure of _______

A. Cast iron
B. Aluminium
C. Brass
D. Zinc alloys
Answer» B. Aluminium
14.

What is the most common etchant used to reveal the grain structure of aluminium alloys?

A. Picral
B. Nital
C. Kellers
D. Adler etchant
Answer» D. Adler etchant
15.

What is the range of misorientation angle in high angle grain boundaries?

A. More than 10°
B. 5 – 10°
C. 1 – 5°
D. Less than 1°
Answer» B. 5 ‚Äö√Ñ√∂‚àö√ë‚àö¬® 10¬¨¬®‚Äö√†√ª
16.

Grain boundary improves ________

A. Electrical conductivity
B. Thermal conductivity
C. Creep strength
D. Toughness
Answer» E.
17.

Which property is deteriorated by increasing grain boundary area?

A. Strength
B. Corrosion resistance
C. Hardness
D. Toughness
Answer» C. Hardness
18.

Which one of the following, is not exhibited by atoms present in the free surface?

A. Improper coordination number
B. Disrupted atomic bonding
C. Higher free energy
D. Less reactive than atoms present in the material
Answer» E.