MCQOPTIONS
Saved Bookmarks
This section includes 8 Mcqs, each offering curated multiple-choice questions to sharpen your Powder Metallurgy knowledge and support exam preparation. Choose a topic below to get started.
1. |
The greater the ______ more will be the driving force for the liquid flow stage in the liquid phase sintering. |
A. | Wetting |
B. | Temperature |
C. | Pressure |
D. | Diffusion |
Answer» B. Temperature | |
2. |
Liquid phase sintering is advantageous over solid phase sintering due to ______ |
A. | Temperature |
B. | Microstructure |
C. | Kinetics |
D. | Economy |
Answer» D. Economy | |
3. |
______ amount of liquid phase must be present to penetrate the adjoining grains. |
A. | Minimum |
B. | Sufficient |
C. | Maximum |
D. | Unlimited |
Answer» C. Maximum | |
4. |
In liquid phase sintering, ______ stresses are developed at the contact point of two particles when the dihedral angle is zero. |
A. | Bending |
B. | Shear |
C. | Tensile |
D. | Compressive |
Answer» E. | |
5. |
______ dihedral angle, will hinder further densification. |
A. | Negative |
B. | Zero |
C. | Positive |
D. | Infinite |
Answer» D. Infinite | |
6. |
Initial particle size must be small for liquid phase sintering. |
A. | True |
B. | False |
Answer» B. False | |
7. |
For liquid phase to sinter successfully, the contact angle should be _______ |
A. | more than 90 |
B. | less than 90 |
C. | equal to 90 |
D. | equal to 0 |
Answer» C. equal to 90 | |
8. |
Which of the following condition should be satisfied for complete penetration of liquid into the grain boundaries? |
A. | <sub>GS</sub> < 0.5 <sub>GB</sub> |
B. | <sub>LG</sub> < 0.5 <sub>GB</sub> |
C. | <sub>GB</sub> < 0.5 <sub>LS</sub> |
D. | <sub>LS</sub> < 0.5 <sub>GB</sub> |
Answer» E. | |