This section includes 5 Mcqs, each offering curated multiple-choice questions to sharpen your Engineering Materials and Metallurgy knowledge and support exam preparation. Choose a topic below to get started.
1. |
The thermal coating thermally grown oxide is formed by the oxidation of _______ |
A. | Silicon |
B. | Magnesium |
C. | Molybdenum |
D. | Aluminum |
Answer» E. | |
2. |
Which crystal structure is the Gamma Double Prime phase of nickel-based superalloy composed of? |
A. | FCC |
B. | BCC |
C. | BCT |
D. | HCP |
Answer» D. HCP | |
3. |
Which phase represents the matrix of the alloy? |
A. | Gamma |
B. | Gamma Prime |
C. | Gamma Double Prime |
D. | Carbide |
Answer» B. Gamma Prime | |
4. |
What is the oxidizing temperature of niobium? |
A. | 100<sup>o</sup>C |
B. | 200<sup>o</sup>C |
C. | 400<sup>o</sup>C |
D. | 600<sup>o</sup>C |
Answer» D. 600<sup>o</sup>C | |
5. |
How can the ductility of tungsten be improved? |
A. | Cold working |
B. | Condensation |
C. | Hot working |
D. | Forming |
Answer» B. Condensation | |