MCQOPTIONS
Saved Bookmarks
This section includes 9 Mcqs, each offering curated multiple-choice questions to sharpen your Corrosion Engineering knowledge and support exam preparation. Choose a topic below to get started.
1. |
Which of the following alloys exhibits intergranular corrosion by steam and marine atmospheres? |
A. | Die-cast zinc alloy |
B. | Duralumin alloy (Al-Cu) |
C. | Both die-cast zinc alloy and duralumin alloy |
D. | Neither die-cast zinc alloy nor duralumin alloy |
Answer» B. Duralumin alloy (Al-Cu) | |
2. |
Which of the following is the best remedy for the Knife-Line attack? |
A. | Heating the welded stabilized steel in the range of 950 F to 1400 F |
B. | Heating the welded stabilized steel in the range of 1400 F to 1900 F |
C. | Heating the welded stabilized steel to 1950 F |
D. | Heating the welded stabilized steel in the range of 1950 F to 2500 F |
Answer» D. Heating the welded stabilized steel in the range of 1950 F to 2500 F | |
3. |
Which of the following is/are the characteristics of the Knife-line attack? |
A. | KLA occurs immediately adjacent to the weld |
B. | KLA occurs in the stabilized steels only |
C. | KLA occurs in the non-stabilized steels only |
D. | KLA occurs in the stabilized steels and it occurs immediately adjacent to the weld |
Answer» E. | |
4. |
What is the abbreviation of KLA regarding intergranular corrosion? |
A. | Knife-Line Attack |
B. | Knight-Line Attack |
C. | Knife-Life Action |
D. | Knight-Life Action |
Answer» B. Knight-Line Attack | |
5. |
The intergranular attack is evident in the resin shell casting but not on the ceramic mold casting. |
A. | True |
B. | False |
Answer» B. False | |
6. |
Carbon pickup during the production of austenitic stainless steels has caused premature failures of intergranular corrosion. |
A. | True |
B. | False |
Answer» B. False | |
7. |
Which of the following is/are the stabilizing elements to minimize intergranular corrosion of stainless steel? |
A. | Niobium |
B. | Columbium |
C. | Titanium |
D. | Niobium, columbium, and titanium |
Answer» E. | |
8. |
Which of the following temperature range is required for commercial solution-quenching treatment? |
A. | 200 F-500 F |
B. | 800 F-1200 F |
C. | 1300 F-1700 F |
D. | 1950 F-2050 F |
Answer» E. | |
9. |
Which of the following is/are the methods to control intergranular corrosion of austenitic stainless steel? |
A. | Employing solution-quenching |
B. | Adding stabilizers |
C. | Lowering the carbon content to below 0.03% |
D. | Employing solution-quenching, adding stabilizers and lowering the carbon content to below 0.03% |
Answer» E. | |