Explore topic-wise MCQs in Corrosion Engineering.

This section includes 14 Mcqs, each offering curated multiple-choice questions to sharpen your Corrosion Engineering knowledge and support exam preparation. Choose a topic below to get started.

1.

Which of the following is the most corrosion-resistant metal at room temperature?

A. Titanium
B. Platinum
C. Gold
D. Tantalum
Answer» E.
2.

The potential generated by two dissimilar metal combinations can change with time.

A. True
B. False
Answer» B. False
3.

What does the square bracket [] in the galvanic series indicates?

A. Most practical metal combinations
B. High corrosion-resistant metals
C. Low corrosion-resistant metals
D. Avoidable metal combinations
Answer» B. High corrosion-resistant metals
4.

Which of the following metal combination has a minimum galvanic effect?

A. Monel and copper
B. Inconel (passive) and Inconel (active)
C. 18-8 stainless steel (active) and 18-8 stainless steel (passive)
D. Titanium and lead
Answer» B. Inconel (passive) and Inconel (active)
5.

Which of the following electrolyte is used for the preparation of a general galvanic series?

A. Polluted seawater
B. Unpolluted river water
C. Polluted river water
D. Unpovlluted seawater
Answer» E.
6.

What is the abbreviation of EMF?

A. Electromagnetic force
B. Electromotive frequency
C. Electromotive force
D. Electrode motive force
Answer» D. Electrode motive force
7.

What is the standard reduction potential value of potassium in the EMF series?

A. +0.337 V
B. -2.925 V
C. -0.763 V
D. -1.662 V
Answer» C. -0.763 V
8.

What is the standard reduction potential value of gold in the EMF series?

A. +1.498 V
B. +1.2 V
C. +0.987 V
D. +0.799 V
Answer» B. +1.2 V
9.

What are the conditions to measure the standard reduction potential of metals against SHE?

A. 2 atm pressure, 25 C temperature, 2M concentration of H<sup>+</sup>
B. 2 atm pressure, 25 C temperature, 1M concentration of H<sup>+</sup>
C. 1 atm pressure, 25 C temperature, 1M concentration of H<sup>+</sup>
D. 1 atm pressure, 25 C temperature, 2M concentration of H<sup>+</sup>
Answer» D. 1 atm pressure, 25 C temperature, 2M concentration of H<sup>+</sup>
10.

Which of the following is the primary characteristic of an electrolyte to form corrosion?

A. Electrical resistivity
B. Thermal resistivity
C. Thermal conductivity
D. Electrical conductivity
Answer» E.
11.

Which of the following will act as cathode and anode respectively in a dry-cell battery?

A. Zinc and carbon
B. Carbon and zinc
C. Magnesium and zinc
D. Zinc and ammonium chloride
Answer» C. Magnesium and zinc
12.

Which of the following is the driving force in galvanic corrosion?

A. Conductivity of electrolyte
B. Crystal structure of metals
C. The potential difference between the two metals
D. Temperature of electrolyte
Answer» D. Temperature of electrolyte
13.

Corrosion of less corrosion-resistant metal is usually increased and the attack of the more corrosion-resistant is decreased in galvanic corrosion.

A. True
B. False
Answer» B. False
14.

1.What is the other name of galvanic corrosion?

A. Bi-metallic corrosion
B. Mono-metallic corrosion
C. Localized corrosion
D. Mono-metallic and localized corrosion
Answer» B. Mono-metallic corrosion