MCQOPTIONS
Bookmark
Saved Bookmarks
→
Casting
→
Continuous Casting in Casting
→
Sharp corners in the casting design also produce t..
1.
Sharp corners in the casting design also produce the problem of sand inclusion in the castings.
A.
True
B.
False
Answer» B. False
Show Answer
Discussion
No Comment Found
Post Comment
Related MCQs
Sharp internal corner of the casting also causes the misrun defect in the casting.
A very large fillet in casting design also may cause shrinkage defects in the casting.
In pattern fillets, the size of a fillet is usually determined by its width.
In casting design, concave junctions are generally added to avoid the effect of sharp corners in the casting.
IN_PATTERN_FILLETS,_THE_SIZE_OF_A_FILLET_IS_USUALLY_DETERMINED_BY_ITS_WIDTH.?$
Sharp internal corner of the casting also causes the misrun defect in the casting.$
A_very_large_fillet_in_casting_design_also_may_cause_shrinkage_defects_in_the_casting.$
To avoid sharp external corners in casting design, rounding of external edges is done in pattern making that termed as radii.
In casting design, concave junctions are generally added to avoid the effect of sharp corners in the casting?
In horizontally parted moulds, a draft is required for vertical as well as for horizontal surfaces of a pattern.