In full annealing, the hypo eutectoid steel is heated from 30°C to 50°C above the upper critical temperature and then cooled$ |
| A. | In still air |
| B. | Slowly in the furnace |
| C. | Suddenly in a suitable cooling medium |
| D. | Any one of these |
| Answer» C. Suddenly in a suitable cooling medium | |