___________ impart hot corrosion resistance in Ni-..
1.
___________ impart hot corrosion resistance in Ni-base superalloys.
A.
Cr
B.
Ti
C.
Mo
D.
Ta
Answer» C. Mo
Show Answer
Discussion
No Comment Found
Post Comment
Related MCQs
When dislocation glide is assisted by vacancy diffusion, resulting creep is known as ___________ creep.
P-N stress is the ___________ obstacle.
Which of the following is an athermal obstacle?
WHICH_OF_THE_FOLLOWING_IS_AN_ATHERMAL_OBSTACLE??$
When dislocation glide is assisted by vacancy diffusion, resulting creep is known as ___________ creep.$
P-N stress is the ___________ obstacle.$
Motion of jogs is the athermal obstacle.
In ultra-fine grain polycrystalline metal, grain boundary sliding is predominant.
Which of the following is a thermal obstacle?
Normalized stress is the ratio of applied stress and ___________
Reply to Comment
×
Name
*
Email
*
Comment
*
Submit Reply